Your English writing platform
Free sign upSuggestions(5)
Exact(51)
The polycrystalline ZGO crystallites had a thickness in the range of 17to2626 nm.
The coating thickness in the range of 5 200 nm was controlled by changing sputtering time.
SEM studies showed the formation of porous films with film thickness in the range of 0 3 μm.
Deposited coatings had thickness in the range of 600 1000 nm as determined by surface profilometry.
The adhesion energy was insensitive to the PEDOT PSS layer thickness in the range of 10 40 nm.
The membrane form of these polymers has a typical thickness in the range of approximately 100 300 μm.
Similar(9)
SEM studies showed the formation of porous films with thicknesses in the range of 0 3 μm.
This solution combines both metals with thicknesses in the range of the fabrication technology.
Homogeneous, crack-free, fully dense coatings with thicknesses in the range of 42 478 μm were obtained.
Individual flow lobes have thicknesses in the range of 1 24 m and many reach widths and lengths exceeding 1000 m.
The coatings consisted of homogeneous single phase cubic TiC with thicknesses in the range of 60 800 nm.
More suggestions(2)
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.
Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com