The specimen was set aside because few H1N1 cases were reported last winter, and the centers routinely concentrate on testing the most prevalent strains.
Although the pre-crack length of the specimen was set to 50 mm to insert the PTFE sheet, an initial crack front is not sufficiently sharp, and overestimation of the G IC value is expected at the first part of the crack propagation.
The estimated power at the specimen was set to 1 mW/mm, as measured with a photodiode (Thorlabs).
In brief, the specimen was set on a computer-controlled microscope stage and observed from the upper side with a charged-coupling device (CCD) camera.
Similar(4)
The cylindrical axis of the specimen is set parallel to that of the glass tube, which is also fixed along the spinning axis by using a collet.
The specimens were set in an intertidal environment and divided into two study groups: one whose bacterial film was removed, and the other whose bacterial film was left intact.
This specimen was used for tear resistance test measurements with a 1 mm nick at point A. The specimens were set up to have the force applied vertically by an Instron 3369 tensile testing machine with a 1 kN load cell (Additional file 1: Figure S1 (Appendix)), at a crosshead displacement speed of 500 mm/min.
A finite element model of the notched specimen was set up for the analysis of the stress field acting during fatigue loading; this allowed a prediction of its fatigue behaviour, which appeared to be in satisfactory agreement with experimental observations.
Related(1)
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com