The ferrite content increases with the solution treatment temperature, but decreases with an increase in Cu.
The sphericity of the aluminides is only slightly increased by the solution treatment.
Upon the solution treatment, Cu2S would be formed on the brass surface as a thin black layer.
The ferrite volume fraction increases with the solution treatment temperature and Al content while decreases with Mn content.
The secondary α lamellar obtained by the solution treatment and aging was responsible for the tensile strength.
This explains the decrease of the high temperature strength of the alloy by the solution treatment tested in hot compression.
Similar(32)
Seeds were not covered by vermiculite, but were exposed to the same light levels as seeds in the solution treatments.
The experimental conditions, such as the amount of MA and NA solutions, pH of the solutions, treatment time, and reaction temperature are investigated.
Samples water-quenched from the solution-treatment temperature of 1350 °C show fault-like features resembling those reported previously as the precursors for the formation of the γ lamellae.
For specimens with the same solution treatment, the a.c.
Compared with the untreated cellulose filled epoxy composites, the NaOH solution treatment increased the tensile strength by 34% and elongation at break by 31%.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com