Adhesion of the coating to the substrate was determined by Scotch tape testing.
From Fig. 6, it was clearly shown that the sheet resistance for the films with mechanical press at 3 MPa and 10 MPa changes from 73.2 Ω/sq to 945.7 Ω/sq and 71.4 Ω/sq to 152.3 Ω/sq, respectively, after tape testing.
Similar(58)
Figure 11 Scotch tape test on Carrara Marble samples.
For adhesion, the adhesion tape test method was done, using a standard 3M tape, 1 1.5 in.
The adhesion of coating is qualitatively assessed by the tape test.
b Photo of UV-cured silver films on glass after tape test.
Besides, the adhesion of UV-cured silver films was also measured by tape test.
The results of the scotch tape test are tabulated in Table 2.
The adhesion performance was measured by 3 M adhesive tape test.
Adhesion of the nickel coating on PET was evaluated by a Scotch® tape test.
Tape test further verifies that there is a strong adhesion between the coating and the substrate.
More suggestions(2)
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com