The flexural strength ranged from 10 to 12 MPa.
The compressive strength ranged from 14 to 31 MPa.
The shear bond strength ranged from 32 to 100 MPa.
The bending strength ranged from 106 to 428 MPa under the influence of porosity.
The compressive strength ranged from 0.2 to 1.1 MPa for different densities.
Across porosity ranged from 51.1% to 80.9%, the compressive strength ranged from 10.0 to 0.6 MPa, the compressive modulus ranged from 14.9 to 12.1 MPa, and the compressive yield strength ranged from 4.25 to 0.42 MPa.
Similar(34)
The tensile strength ranges from 0.021 to 0.059 MPa.
The compressive strength ranges from 0.39 to 0.68 MPa.
UHDCC had the compressive strength ranging from 45.9 MPa to 121.5 MPa.
These highly porous Si3N4 ceramics showed fine compressive strength ranging from 6.7 MPa to 59.9 MPa.
Prepared beads were spherical with crushing strength ranging from 182 to 1073 g.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com