Solvent thermal method was employed to deposit Cu2S nanoparticles.
First, Fe3O4 nanospheres were made by solvent thermal method.
PbS CQDs with different ligands were synthesized by a solvent thermal method reported previously [23].
Figure 1 illustrates the XRD pattern of the synthesized Cu2S after 5 h solvent thermal reaction.
Figure 2 SEM images of the graphite paper surface a before and b after 5 h solvent thermal treatment.
After the solvent thermal treatment, a great amount of Cu2S nanocrystal particles was deposited onto the surface of graphite with spread dispersion.
Similar(47)
Manganese indium sulfide (MnIn2S4) urchins were successfully synthesized via a simple mixed-solvent thermal route in "aqueous solution water-immiscible organic solution water-immiscible
These polymers exhibited good solubility in common organic solvents, thermal stability up to 400 °C, and facile film formation.
Surface temperature histories are studied for CO2 absorption into four solvents; thermal effects of absorption are responsible for the diverging flow that accompanies absorption.
Fig. 1 XRD patterns of the FTO substrate before solvent-thermal growth and after.
The solvent-thermal synthesis was conducted at 140 °C for 6 h.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com