Your English writing platform
Discover LudwigExact(2)
PMMA shows poor adhesion for evaporated inorganic coatings.
The embedding technique may find utility in functionalizing polymer surfaces that do not withstand high temperature coating methods, which provide poor adhesion for paint films, or where flexibility of the polymer needs to be maintained.
Similar(58)
However, for some industrial applications, the poor adhesion of PTFE to other materials is a disadvantage.
It is found that the acidic electrolyte is not suitable for depositing NiTe2 thin films as proven by the inappropriate reduction range and poor adhesion of films.
All the described methods suffer from the poor adhesion of AuNP to the substrate surface [7].
Poor adhesion of inhomogeneous lumpy transfer layer in Group 2 showed an intermediate wear rate.
One of the major problems for the deposition of cubic boron nitride c-BN) films onitride c-BN high speed steels(HHS) is the poor adhesion ofilms film tonthe substrate.
However, poor adhesion was obtained for arc-evaporated zirconium films deposited on epoxy powder coatings in the prototype machine.
The presence of an optimum initial film thickness seems to be a balance between solvent surface damage for very thin films, and poor adhesion to the substrate for thicker films.
Poor adhesion is a recurrent problem for the wider use of diamond-like carbon (DLC) coatings in industrial applications.
The industrial use of linear low density polyethylene (LLDPE) and poly ethylene terephthalate) (PET) films are limited because of undesirable properties of the polymer surface, for example, poor adhesion, printability, and gas barrier properties.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com