Exact(8)
The albumin-water and albumin-natural rubber plastics showed higher onset degradation temperatures.
The nanocomposites displayed a little higher onset degradation temperature than pure polymer by 7 11 °C.
The onset degradation temperatures of the polymers were greater than that of fluorescein.
The onset degradation temperatures (Td,onset) ranged between 115 and 148 °C, and were obtained by thermogravimetric analysis.
The CS/EMImC-Co-EP membranes show excellent thermal stability with onset degradation temperature high above 200 °C.
The thermograms of untreated P. pinnata seed hull fibres and isolated cellulose fibres as shown in Fig. 5 have onset degradation temperature of 200 and 270 °C, respectively.
The isothermal TGA tests were performed at four different temperatures slightly above 370 °C, which corresponds to the onset degradation temperature in a dynamic TGA thermogram.
On the other hand, the onset degradation temperature of the SF electrospun was not significantly altered by inclusion of ferrite nanoparticles.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com