The modulation period of the deposited CrAlSiN/TiVN coatings was 9 nm.
At a modulation period of 10 nm, the reduction of the dissipated energy and the energy dissipated ratio were observed.
With the increase of Srs, the modulation period of the coatings decreased from 21.9 nm to 2.40 nm.
For λTi/TiN=1 3, the hardness enhancement appears in the films with the modulation period of 20 70 nm.
The maximum hardness and oxidation temperature can reach 31 GPa and 630 °C, respectively, at the modulation period of 150 nm.
It exhibited better anti-oxidation behavior than either the monolayered CrN or multilayered CrN/AlN coating with modulation period of 20 nm.
Similar(26)
XRD, AES, Nanoindenter and profiler were employed to investigate the influence of modulation period on microstructure and mechanical properties of the coatings.
The modulation periods of the multilayer coatings was evidenced by transmission electron microscopy (TEM).
The layers were designed with modulation periods of approximately 13 nm, up to a total thickness of 2.8 μm.
CrN/AlN multilayer coatings with modulation periods of 4 nm and 20 nm were fabricated on silicon (001) substrates by RF magnetron sputtering technique.
TaN/a-CNx multilayer films with modulation periods of 8.5 12 nm are deposited on Si wafers and titanium alloy substrate using direct current magnetron sputtering.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com