The elongation at break decreased from 11 to 4% upon addition of carbon nanotubes, however, reasonable flexibility was retained.
Likewise, the elastic modulus increased from 70 to 524 MPa, the stress at break increased from 8to2828 MPa while the strain at break decreased from 820 to 370%.
The double bond density primarily governed the mechanical performance of CO2-UV-WPU, when it increased from 0.93 mmol/g to 2.4 mmol/g, the tensile strength increased from 29 MPa to 67 MPa, while elongation at break decreased from 150% to 9.6%, accompanied by the reduction of maximum water swelling percentage from 26.7% to 14.5%.
Similar(57)
Elongation at break decreased drastically from 1000% to 20% while strength at break remained approximately constant.
Following PDT, pO2 increased from 21.5±2.7 mmHg (baseline) to 23.8±3.2 mmHg (in the irradiation break), decreased to 17.7±6.7 mmHg (15 min/2 h) followed by a slight decrease after 24 h in surrounding tissue.
The tensile strength and tensile strain at break decreased.
When the synaptic density was reduced to a quarter of its initial value, while maintaining a constant I/E ratio, the critical velocity at which motion anticipation broke down decreased from ≥1 mm s−1 to ∼0.5 mm s−1.
Consequently, the elongation at break of the PSCMS-g-DGEBA/AuNPs-PSNPs 0.1 1 membranes was decreased from 4.6 to 3.1 % with the increasing filler content.
Opposition decreased from 49 percent to 40 percent.
This has decreased from value of $1.15m.
The black population has decreased from 11%to8%8%.
Write better and faster with AI suggestions while staying true to your unique style.
Since I tried Ludwig back in 2017, I have been constantly using it in both editing and translation. Ever since, I suggest it to my translators at ProSciEditing.

Justyna Jupowicz-Kozak
CEO of Professional Science Editing for Scientists @ prosciediting.com